CNS-SCC13
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Limite d'élasticité (Mpa) | Contrainte de traction (Mpa) | Élongation (%) |
|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) ≦0.08 | Si(%)(%) ≦2.0 | Mn(%)(%) ≦2.0 | P(%)(%) ≦0.04 | S(%)(%) -0,04 | Ni(%)(%) 8.0-11.0 | Cr(%)(%) 18,0-21,0 | Limite d'élasticité (Mpa)(%) ≧185 | Contrainte de traction (Mpa)(%) ≧440 | Élongation (%)(%) ≧30 |
Applications
- Fonte en acier inoxydable
Code pays
- CNS
Norme
- 4000
Type d'acier
- SCC13
Type d'acier associé
| Type d'acier | Norme | Code pays | Suite | SCC13 | 4000 | CNS | Suite | SCS13A | 4000 | CNS | Suite | ZG0Cr-18Ni9 | 2100 | GB | Suite | SCS13A | G5121 | JIS | Suite | CF-8 | A351 A743 A744 | ASTM | Suite | G-X6Cr-Ni18-9 | 17445 | DIN | Suite |
|---|