CNS-SCS12
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Limite d'élasticité (Mpa) | Contrainte de traction (Mpa) | Élongation (%) |
|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) ≦0.2 | Si(%)(%) ≦2.0 | Mn(%)(%) ≦2.0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni(%)(%) 8.0-11.0 | Cr(%)(%) 18.0-20.0 | Limite d'élasticité (Mpa)(%) ≧205 | Contrainte de traction (Mpa)(%) ≧480 | Élongation (%)(%) ≧28 |
Applications
- Fonte en acier inoxydable
Code pays
- CNS
Norme
- 4000
Type d'acier
- SCS12
Type d'acier associé
| Type d'acier | Norme | Code pays | Suite |
SCS12 |
4000 | CNS | Suite |
ZG1Cr-18Ni9 |
2100 | GB | Suite |
SCS12 |
G5121 | JIS | Suite |
CF-20 |
A743 | ASTM | Suite |
G-X10Cr-Nil8-8 |
17445 | DIN | Suite |
|---|