CNS-SCS18
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Contrainte de rendement (Mpa) | Contrainte de traction (Mpa) | Allongement (%) |
|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) ≦0,2 | Si(%)(%) ≦2,0 | Mn(%)(%) ≦2,0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) 19,0-22,0 | Cr (%)(%) 23,0-27,0 | Contrainte de rendement (Mpa)(%) ≧195 | Contrainte de traction (Mpa)(%) ≧450 | Allongement (%)(%) ≧28 |
Applications
- Fonderies en acier inoxydable
Code pays
- CNS
Norme
- 4000
Type d'acier
- SCS18
Type d'acier associé
| Type d'acier | Norme | Code pays | Suite |
SCS18 |
4000 | CNS | Suite |
SCS18 |
G5121 | JIS | Suite |
CK-20 |
A743 | ASTM | Suite |
|---|