| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Mo(%) | Limite d'élasticité (Mpa) | Contrainte de traction (Mpa) | Élongation (%) |
|---|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) 0,16-0,24 | Si(%)(%) ≦1.5 | Mn(%)(%) ≦1.0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni(%)(%) ≦1.0 | Cr(%)(%) 11.5-14.0 | Mo(%)(%) ≦0,5 | Limite d'élasticité (Mpa)(%) ≧390 | Contrainte de traction (Mpa)(%) ≧590 | Élongation (%)(%) ≧16 |
Applications
- Fonte en acier inoxydable
Code pays
- CNS
Norme
- 4000
Type d'acier
- SCS2
Type d'acier associé
| Type d'acier | Norme | Code pays | Suite | SCS2 | 4000 | CNS | Suite | ZG2Cr13 | 2100 | GB | Suite | SCS2 | G5121 | JIS | Suite | CA-40 | A743 | ASTM | Suite | G-X20Cr14 | 17445 | DIN | Suite |
|---|