CNS-SCS20
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Mo(%) | Cu(%) | Limite d'élasticité (Mpa) | Contrainte de traction (Mpa) | Élongation (%) |
|---|---|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) ≦0.03 | Si(%)(%) ≦2.0 | Mn(%)(%) ≦2.0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni(%)(%) 12.0-16.0 | Cr(%)(%) 17,0-20,0 | Mo(%)(%) 1,75-2,75 | Cu(%)(%) 1.0-2.5 | Limite d'élasticité (Mpa)(%) ≧175 | Contrainte de traction (Mpa)(%) ≧390 | Élongation (%)(%) ≧33 |
Applications
- Fonte en acier inoxydable
Code pays
- CNS
Norme
- 4000
Type d'acier
- SCS20
Type d'acier associé
| Type d'acier | Norme | Code pays | Suite |
SCS20 |
4000 | CNS | Suite |
SCS20 |
G5121 | JIS | Suite |
|---|