| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Cu(%) | Al(%) | Tegangan Luluh (Mpa) | Tegangan Tarik (Mpa) | Pemanjangan (%) |
|---|---|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) ≦0.1 | Si(%)(%) ≦0.5 | Mn(%)(%) ≦1.0 | P(%)(%) ≦0.03 | S(%)(%) ≦0,015 | Ni(%)(%) 58.0-63.0 | Cr(%)(%) 21.0-25.0 | Cu(%)(%) ≦1.0 | Al(%)(%) 1.0-1.7 | Tegangan Luluh (Mpa)(%) ≧195 | Tegangan Tarik (Mpa)(%) ≧550 | Pemanjangan (%)(%) ≧30 |
Aplikasi
- Lembar, Plat, dan Batang Superalloy Tahan Korosi dan Tahan Panas
Kode Negara
- CNS
Tipe Baja
- NCF601
Tipe Baja Terkait
| Tipe Baja | Kode Negara | Lagi | NCF601 | CNS | Lagi | NCF601 | JIS | Lagi |
|---|