CNS-SCMnCr-M3A
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | Tegangan Luluh (Mpa) | Tegangan Tarik (Mpa) | Pemanjangan (%) |
|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) 0.3-0.4 | Si(%)(%) 0.3-0.6 | Mn(%)(%) 1.2-1.6 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Cr(%)(%) 0.3-0.7 | Mo(%)(%) 0.15-0.35 | Tegangan Luluh (Mpa)(%) ≧540 | Tegangan Tarik (Mpa)(%) ≧740 | Pemanjangan (%)(%) ≧9 |
Aplikasi
- Paduan Baja Karbon Kekuatan Tarik Tinggi dan Paduan Baja Rendah untuk Struktur
Kode Negara
- CNS
Standar
- 7145
Tipe Baja
- SCMnCr-M3A
Tipe Baja Terkait
| Tipe Baja | Standar | Kode Negara | Lagi | SCMnCr-M3A | 7145 | CNS | Lagi | SCMnCr-M3A | G5111 | JIS | Lagi |
|---|