CNS-SFVAF5C
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | Tegangan Luluh (Mpa) | Tegangan Tarik (Mpa) | Pemanjangan (%) |
|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) ≦0.25 | Si(%)(%) ≦0.5 | Mn(%)(%) 0.3-0.6 | P(%)(%) ≦0.03 | S(%)(%) ≦0.03 | Cr(%)(%) 4,0-6,0 | Mo(%)(%) 0.45-0.65 | Tegangan Luluh (Mpa)(%) ≧345 | Tegangan Tarik (Mpa)(%) 550-730 | Pemanjangan (%)(%) ≧18 |
Aplikasi
- Paduan Baja Forging untuk Bejana Tekanan untuk Layanan Suhu Tinggi
Kode Negara
- CNS
Tipe Baja
- SFVAF5C
Tipe Baja Terkait
| Tipe Baja | Kode Negara | Lagi |
SFVAF5C |
CNS | Lagi |
SFVAF5C |
JIS | Lagi |
F5A |
ASTM | Lagi |
X12CrMo7 |
DIN | Lagi |
|---|