CNS-SCH12
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr(%) | Mo(%) | Vloeigrens (Mpa) | Treksterkte (Mpa) | Rek (%) |
|---|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) 0,2-0,4 | Si(%)(%) ≦0.2 | Mn(%)(%) ≦0.2 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) 8.0-12.0 | Cr(%)(%) 18.0-23.0 | Mo(%)(%) ≦0,5 | Vloeigrens (Mpa)(%) ≧235 | Treksterkte (Mpa)(%) ≧490 | Rek (%)(%) ≧23 |
Toepassingen
- Hittebestendige staalgietstukken
Landcode
- CNS
Standaard
- 4002
Staaltype
- SCH12
Gerelateerd Staaltype
| Staaltype | Standaard | Landcode | Meer |
SCH12 |
4002 | CNS | Meer |
SCH12 |
G5122 | JIS | Meer |
HF |
A297 | ASTM | Meer |
G-X40Cr-NiSi22-9 |
17465 | DIN | Meer |
|---|