| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr(%) | Mo(%) | Vloeigrens (Mpa) | Treksterkte (Mpa) | Rek (%) |
|---|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) 0,25-0,5 | Si(%)(%) ≦1.75 | Mn(%)(%) ≦2,5 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) 12.0-14.0 | Cr(%)(%) 23.0-26.0 | Mo(%)(%) ≦0,5 | Vloeigrens (Mpa)(%) ≧235 | Treksterkte (Mpa)(%) ≧490 | Rek (%)(%) ≧8 |
Toepassingen
- Hittebestendige staalgietstukken
Landcode
- JIS
Standaard
- G5122
Staaltype
- SCH13A