CNS-SCH22
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Mo(%) | Yield stress (Mpa) | Tensile stress (Mpa) | Pagpahaba (%) |
|---|---|---|---|---|---|---|---|---|---|---|
| C(%)(%) 0.35-0.45 | Si(%)(%) ≦1.75 | Mn(%)(%) ≦1.5 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni(%)(%) 19.0-22.0 | Cr(%)(%) 23.0-27.0 | Mo(%)(%) ≦0.5 | Yield stress (Mpa)(%) ≧235 | Tensile stress (Mpa)(%) ≧440 | Pagpahaba (%)(%) ≧8 |
Mga Aplikasyon
- Mga Casting na Bakal na Lumalaban sa Init
Code ng Bansa
- CNS
Pamantayan
- 4002
Uri ng Bakal
- SCH22
Kaugnay na Uri ng Bakal
| Uri ng Bakal | Pamantayan | Code ng Bansa | Higit pa |
SCH22 |
4002 | CNS | Higit pa |
ZG40Cr25-Ni20 |
8492 | GB | Higit pa |
SCH22 |
G5122 | JIS | Higit pa |
HK40 |
A351 | ASTM | Higit pa |
G-X40Cr-NiSi25-20 |
17465 | DIN | Higit pa |
|---|